Program: KIC Compact Tension Specimen Data Date: Mon, Oct 12, 2026 Time: 3:37 PM Course: C02CD Section: C02CD Material: 6061-T6 Precrack Data: Loading wave Shape: Haversine Low: 0.50 kN High: 8.50 kN Frequency: 4.00 Hz Number of cycles: 17000 Specimen Measurements: Thickness (B or t): 25.38 mm Width (W): 50.91 mm Crack tip to end (z): 27.17 mm 26.92 mm 27.56 mm 25.74 mm 27.14 mm 27.81 mm